Master

The master is the model of the part that liquid silicone is poured around to form the vacuum casting tool.

Every Master article of the Vacuum Casting Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The master is the model of the part that liquid silicone is poured around to form the vacuum casting tool. Once the silicone cures, the block is cut open and the master comes out, leaving a cavity in its shape. Every copy inherits the master’s form and surface. Renishaw notes that masters come from several 3D printing processes, stereolithography being the most common.

Source of Size

Every cast size starts from the master, and the casting step adds a smaller error of its own. A 2020 study cast one battery cover from 3 printed masters. On a dimension drawn at 49.84 mm (1.962 in), the FDM master measured 0.488 mm (0.019 in) short. The SLA master came out 0.137 mm (0.005 in) long and the MJF master 0.308 mm (0.012 in) long. The casting step added under 0.05 mm (0.002 in) on the FDM and SLA series. The cast parts spread over 0.71 mm (0.028 in), set mostly by the master.
Read More

Surface Transfer

A cast copy follows its master’s surface closely. The study measured master roughness of Ra 22.075 µm (869 µin) for FDM and 4.075 µm (160 µin) for SLA. The MJF master read Ra 14.548 µm (573 µin). The cast parts came out between 1.84 % and 9.62 % smoother than their masters. A buyer who needs a smooth copy therefore asks for a smoothed master. The copy is then checked against a measured value.

Scale Factor

Resin shrinks, so the master is usually made larger than the drawing. For a shrinkage fraction s, the master is made 1 ÷ (1 − s) times the drawn size. For a 0.7 % resin, a 100 mm (3.94 in) feature is mastered at 100.70 mm (3.965 in). For a 0.3 % resin it becomes 100.30 mm (3.949 in). Scaling uniformly corrects only the mean loss. The first article decides whether single features on the master are corrected.

Contact Materials

Whatever coats the master touches the uncured silicone. Vacusil 2000’s sheet lists adhesive tapes, waxes and paints among the materials that can inhibit its cure. A patch test of the master’s coating and tapes comes before the first pour. During the pour, air trapped against the master’s flat faces or under its overhangs becomes a void in the tool. A void against the master’s surface repeats on every copy.

Tool Sequence

Each silicone tool is cast fresh around the master, and each is a separate cavity. The master stays in the frame until the silicone cures and the block is cut. A plan of 4 tools from one master therefore takes about 4 silicone cures in sequence. A set of 4 master copies turns the same work into 1 cure in parallel. Damage to the master while a block is cut sends the plan back to the beginning.

Material Quantities

The master also sets how much material each step needs. Silicone needed equals frame volume less master volume, with an allowance for the bowl. The 2020 study sized each resin pour at about 1.3 times the weight of its master. Time starts from the master too. Renishaw quotes first parts within 24 hours of having a master. Formlabs estimates about 10 days for a full job from master to finished castings.

Ownership

A silicone tool is a consumable, normally spent on the order it was made for. Reorders begin again at the master, with fresh tools and fresh first parts. The master is the asset that carries between deliveries, so who keeps it is settled in writing. When a part moves to an injection mold, the master stays a reference for shape. Steel or aluminum tools are cut from CAD.

Process Choice

A 2020 study advises making replacement parts with the same additive process as the original master. Its SLA and MJF covers did not fit the enclosure, because one dimension came out too large to clear the cavity. Measuring the master before the silicone is poured costs minutes and removes the largest source of error. A drawing note can name the master process and the measured size of each critical feature on it.

Vacuum Casting Defects in a Batch Traced to Their Cause

A vacuum casting defect points to its cause by where it sits on the part and which castings of the batch show it, from one wet pour to a mold near its end.

The List of Casting Defects and the Cause Behind EachVacuum casting defects trace to six causes: moisture in the components, air folded in during mixing and pouring, a mixing ratio upset by weighing or crystallization, a mold or master fault copied into every part, a cure or demold cut short, and a silicone mold wearing out over the run. The table pairs the defects named in the opened documents with those causes and with what a buyer or inspector sees.

Color Matching a Vacuum Cast Batch to a RAL or Pantone Reference

A vacuum cast color is fixed as a weighed recipe on an approved first article, measured with an agreed formula and tolerance, and repeated for every pour.

How a Vacuum Cast Batch Is Matched to a RAL or Pantone ColorA vacuum cast batch is matched to a reference by pigmenting each pour with a paste dosed within the resin maker's limit, casting a first part, measuring it against the reference under agreed conditions, adjusting the recipe, and then holding that recipe for every pour, with parts checked against the approved first article. Renishaw describes the casting system as producing typically 30 to 50 color-matched parts from a single mold, which is the batch size the recipe has to stay steady over.

Painting and Texturing Vacuum Cast Parts After Demold

A cast urethane part is painted only after its release agent is washed off and its surface keyed, with flexible coatings on parts that bend.

Painting Vacuum Cast Parts Step by StepA vacuum cast part is painted by removing the release agent, keying and degreasing the surface, applying an adhesion promoter where the substrate calls for one, priming, and then applying the color and clear coats, with flexible additives in every layer when the part bends. The car refinish makers write the sequence most completely, because they paint new plastic parts every day.

Overmolding and Inserts in Vacuum Casting Step by Step

Inserts in a cast part are held by knurls and undercuts, located on pins in the silicone, and surrounded by resin mixed and poured under vacuum.

The Vacuum Casting Steps for a Part With InsertsA vacuum cast part with molded-in inserts is made in eight steps: the insert is chosen and shaped for mechanical retention, the master is prepared so the mold can locate it, the insert's surface is prepared, it is placed in the opened silicone mold, the mold is closed and preheated, the resin is degassed and mixed under vacuum, the mold is filled and vented, and the part is cured and demolded around the insert. An overmolded part adds a second mold and a second pour.

Making the Master Pattern for Vacuum Casting From SLA or CNC

The master is finished, sealed and fitted with its parting line, gate and risers before the silicone is poured, because the mold copies every mark into the batch.

What the Master Pattern Has to Deliver Before the Silicone Is PouredA master pattern for vacuum casting is the physical original from which the silicone mold is cast, and the mold reproduces it so faithfully that every cast part inherits its shape, its surface and its faults. Loughborough University's vacuum casting guide puts it plainly: the mold replicates the master extremely faithfully, so the master's surface finish and accuracy are what the moldings will have.

Surface Finish of Vacuum Cast Parts and How the Master Sets It

A vacuum cast part copies its master's roughness and comes out slightly smoother, so the finish is specified and measured on the master before the mold is poured.

How Closely a Vacuum Cast Surface Follows Its MasterA vacuum cast part's surface roughness is set by its master within about a tenth of the master's value, in the two studies on file. In the 2020 study by Mustafa and co-authors, parts cast from FDM, SLA and multi jet fusion (MJF) masters all came out smoother than the master, by 1.84 %, 9.62 % and 6.09 % respectively.

Rubber-Like Polyurethane Resins From Shore 30 A to 90 A

A rubber-like urethane is specified by grade, hardness method and a tested service temperature, because hardness alone leaves strength and heat behavior open.

Rubber-Like Vacuum Casting Grades and the Hardness Each CoversRubber-like vacuum casting resins are two- or three-component polyurethanes that cure in a silicone mold to an elastomer, with a Shore A hardness chosen for the part. The variable-hardness systems reach the range by adding a third component to a fixed A:B pair.

When a Vacuum Cast Run Should Move to an Injection Mold

Silicone molds carry a pilot, and a hard tool follows once the quantity, colors and repeat orders outgrow a handful of tools.

Where Silicone Tools Stop and the First Injection Mold StartsInjection molds are rated in classes by the construction they are built to and the cycles they are expected to give. The classification belongs to the plastics industry's trade body, PLASTICS, formerly the Society of the Plastics Industry, and its own text was not opened for this piece.

Silicone Molds, Pours and Lead Time for a Vacuum Cast Batch

A batch needs one silicone mold per set of copies, per resin and per color, and pours run one at a time through the chamber.

How Many Silicone Molds a Vacuum Cast Batch NeedsThe tool count is the quantity divided by the copies one tool gives, rounded up. Renishaw states that a mold can produce up to 50 parts before retooling and typically between 30 and 50 colour matched parts.

Degassing Silicone and Resin in Vacuum Casting

Each resin component is evacuated alone for about ten minutes, the silicone twice, and the air returns before the pot life ends.

Why Silicone and Resin Are Degassed Under VacuumMixing puts air into any liquid. Stirring two viscous components together folds the surface into the bulk, and a general guide from the mold supplier ArtMolds puts the air picked up by mixing at 5 % to 20 % of the volume, calling it the primary cause of bubbles in cast parts.

Wall Thickness Limits for Vacuum Cast Polyurethane Parts

Each casting resin carries a maximum thickness printed by its maker, and every property on its sheet describes a specimen of one stated thickness, not the whole part.

Maximum Casting Thickness as the Maker Prints ItSeveral Sika sheets print a line titled maximum casting thickness, and Sika's text for PX522 and PX523 words the same idea as parts until 10 mm or until 100 mm thickness by vacuum casting in silicone molds. Renishaw's resin sheets for 6230 and 8263 print no such line.

Linear Shrinkage of Cast Polyurethane Resins Per 100 mm

Printed shrinkage belongs to one bar and one cure, so the master is scaled from it as a starting point and the first article confirms each critical dimension.

Linear Shrinkage Read as Millimeters Per MeterLinear shrinkage is the fractional loss in length between the mold cavity and the cured part. A resin that fills a cavity 100 mm long and cures into a part that measures 99.3 mm has shrunk by 0.7 percent, which is the same as 7 mm per meter.

Dimensional Accuracy of Vacuum Cast Parts From SLA, FDM and MJF Masters

A cast copy follows its master within a small fraction of a millimeter, and the printed master is the larger source of error against the drawing.

How Accurate Vacuum Cast Parts Are in a Published StudyThe authors cast a battery cover for an enclosure, a thin-walled part 1.5 mm (0.059 in) thick with two measured dimensions: section A at 26.84 mm (1.057 in) and section B at 49.84 mm (1.962 in), both from the CAD model. They made three masters of it by three additive processes: fused deposition modeling (FDM) in ABS, stereolithography (SLA) in a detailed white resin, and multi-jet fusion (MJF) in polyamide.

Silicone Rubber for Vacuum Casting Molds

Mold silicone is an addition-cure rubber chosen for hardness and resin resistance, checked against every material it touches, and treated as a consumable.

Silicone Rubber as the Mold Material in Vacuum CastingA mold silicone is a two-component liquid rubber that is poured round a master, cured at room temperature or a little above, and cut open to release the master. Renishaw describes Vacusil 2000 as a two-component addition-cure liquid silicone rubber designed for mold making, curing at room temperature to a translucent, high-strength elastic rubber, and names vacuum casting of polyurethane resins among its uses.

Send the Drawing of Your Cast Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Vacuum Casting chosen.

Request a Quote