Data Sheet

A data sheet is the maker's document for one casting grade, stating how to process it and what the cured material measured.

Every Data Sheet article of the Vacuum Casting Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A data sheet is the maker’s document for one casting grade, stating how to process it and what the cured material measured. Sika calls its versions product or technical data sheets, and Renishaw issues one per vacuum casting resin and per mold silicone. The values are typical figures from laboratory specimens. Sika warns that real results can differ under conditions it does not control. Renishaw asks users to run enough tests to establish suitability for the intended part.

Processing Block

The first half of a casting sheet is a set of instructions with numbers attached. It gives the mix ratio by weight and the pot life, each pot life tied to a mass and a temperature. The mold temperature is 70 °C (158 °F) on every resin sheet in these resources. Then come the demold time, often split by wall thickness, the maximum casting thickness where one is printed, and the post-cure. Handling lines close the block: component temperature, degassing time, crystals after cold storage and containers closed at once against moisture.
Read More

Cure Footnote

Most property values on a Sika sheet carry a footnote letter naming the cure the specimen had before the test. On the PX331 sheet the capital A after Shore D 86 is such a marker. It points to 1 hour at 70 °C (158 °F) plus 16 hours at 80 °C (176 °F). Read as a scale letter, it would turn a rigid plastic into a soft rubber. Renishaw’s sheets for 6230, 8263 and 8020-2 list no post-cure, so their figures describe the part as demolded. A part shipped without the cure in the footnote is a different material state from the one in the table.

Specimen and Method

Every property belongs to a specimen of a stated size, measured by a stated method. Renishaw’s heat deflection bar measures 110 × 12.7 × 6.4 mm (4.33 × 0.50 × 0.25 in). Sika’s ISO 75A figures name no bar at all. Shrinkage sits on named bars, such as 3 × 50 × 250 mm (0.12 × 1.97 × 9.84 in) for PX205. Pot life is read on one cup, 200 g (7.1 oz) at 23 °C (73 °F) for PX331. A part of another thickness, mass or shape is described only as far as it matches those conditions.

Comparison Across Makers

A maker’s sheets compare its own grades fairly, and other makers’ grades badly. Glass transition appears under ISO 11359 on PX331 and by thermomechanical analysis on Renishaw 6230. PX 223 HT names a third document, ASTM E1545. Impact resistance appears as Charpy on one sheet and Izod on another, with different notches. Heat deflection carries a method letter on some sheets and no method on the 8263 sheet. A comparison holds only where both values share the method, the specimen and the cure.

Edition and Age

Each sheet carries an issue date or a version, and the dates in these resources run from 2015 to 2026. Sika’s PX523 sheet marks 2 electrical lines with the word OUTDATED. Renishaw’s brochure lists resin 8263 with a 5V flame claim that its own sheet does not make. Where 2 documents of one maker disagree, the sheet of the grade is the conservative reading. The buyer then asks the maker for the current value.

Known Gaps

Several answers a designer needs sit outside every sheet on file. Creep, fatigue and heat aging are absent from all of them. None defines a minimum wall or a flow length. None says whether the maximum casting thickness means a nominal wall or a local boss. Most print no flame rating. Wacker’s page for ELASTOSIL M 4601 gives a handful of figures and points to a full technical data sheet.

Typical Value

Much of a sheet is printed as typical, and the word carries a limit of its own. Renishaw gives shrinkage as typical 0.3 % for 6230 and 8263 without naming a bar. Whether such a number was measured on a bar, a part or estimated is not stated. A typical value is a starting point for a plan. It is never a guaranteed property of a delivered copy.

Quote Use

A sheet value becomes useful in a request when it travels with its conditions. The buyer names the grade, the sheet edition, the method behind the figure, its cure and its specimen thickness. A first article cast in that grade and cured as the sheet describes then shows whether the delivered part matches the printed number.

Painting and Texturing Vacuum Cast Parts After Demold

A cast urethane part is painted only after its release agent is washed off and its surface keyed, with flexible coatings on parts that bend.

Painting Vacuum Cast Parts Step by StepA vacuum cast part is painted by removing the release agent, keying and degreasing the surface, applying an adhesion promoter where the substrate calls for one, priming, and then applying the color and clear coats, with flexible additives in every layer when the part bends. The car refinish makers write the sequence most completely, because they paint new plastic parts every day.

ISO 527 Tensile Values on Polyurethane Casting Resin Data Sheets

A tensile value on a casting resin sheet belongs to standard bars after one stated cure, so a requirement on parts is set on bars cast and cured with the batch.

What ISO 527 Covers on a Casting Resin Data SheetISO 527 is the international method for tensile properties of plastics, and casting resins fall inside it. The scope of ISO 527-1, as published by the Estonian standards body, sets out the general principles for determining tensile strength, tensile modulus and other aspects of the stress and strain relationship under defined conditions.

ISO 179 and ISO 180 Impact Strength on Cast Resin Data Sheets

Impact values on cast resin sheets are comparisons tied to method, notch, specimen and cure, so a part's toughness is set by tests on batch bars or the part.

What ISO 179 and ISO 180 Measure on a Cast ResinBoth standards measure how much energy a pendulum hammer loses breaking a small bar of plastic at a high strain rate. ZwickRoell, a maker of the testing machines, describes the principle in its pages on both methods: a hammer of specified energy and drop height strikes the specimen, does not swing back to its starting height, and the height difference is taken as the energy absorbed.

PP-Like and PE-Like Polyurethane Casting Resins for Vacuum Casting

PP-like and PE-like urethanes trade stiffness for elongation by grade, and their heat figures depend on cure, so the first cast part is tested in its real duty.

What PP-Like and PE-Like Mean on a Casting Resin Data SheetA PP-like or PE-like grade is a two- or three-component polyurethane formulated so that a part cast in a silicone mold behaves, in hand and in a snap fit, more like polypropylene or polyethylene than like a stiff ABS replica. The makers say so in their own words.

Demolding and Post-Curing Vacuum Cast Parts

Each grade prints its own demold time and its own post-cure, and thin or long parts are supported in the oven while it runs.

Demolding Vacuum Cast Parts at 70 °CDemolding means opening the silicone tool and taking the copy out once the resin has gelled and hardened far enough to hold its form. In every sheet on file the tool stays at 70 °C (158 °F) in the oven for that time.

Degassing Silicone and Resin in Vacuum Casting

Each resin component is evacuated alone for about ten minutes, the silicone twice, and the air returns before the pot life ends.

Why Silicone and Resin Are Degassed Under VacuumMixing puts air into any liquid. Stirring two viscous components together folds the surface into the bulk, and a general guide from the mold supplier ArtMolds puts the air picked up by mixing at 5 % to 20 % of the volume, calling it the primary cause of bubbles in cast parts.

Wall Thickness Limits for Vacuum Cast Polyurethane Parts

Each casting resin carries a maximum thickness printed by its maker, and every property on its sheet describes a specimen of one stated thickness, not the whole part.

Maximum Casting Thickness as the Maker Prints ItSeveral Sika sheets print a line titled maximum casting thickness, and Sika's text for PX522 and PX523 words the same idea as parts until 10 mm or until 100 mm thickness by vacuum casting in silicone molds. Renishaw's resin sheets for 6230 and 8263 print no such line.

Linear Shrinkage of Cast Polyurethane Resins Per 100 mm

Printed shrinkage belongs to one bar and one cure, so the master is scaled from it as a starting point and the first article confirms each critical dimension.

Linear Shrinkage Read as Millimeters Per MeterLinear shrinkage is the fractional loss in length between the mold cavity and the cured part. A resin that fills a cavity 100 mm long and cures into a part that measures 99.3 mm has shrunk by 0.7 percent, which is the same as 7 mm per meter.

Dimensional Accuracy of Vacuum Cast Parts From SLA, FDM and MJF Masters

A cast copy follows its master within a small fraction of a millimeter, and the printed master is the larger source of error against the drawing.

How Accurate Vacuum Cast Parts Are in a Published StudyThe authors cast a battery cover for an enclosure, a thin-walled part 1.5 mm (0.059 in) thick with two measured dimensions: section A at 26.84 mm (1.057 in) and section B at 49.84 mm (1.962 in), both from the CAD model. They made three masters of it by three additive processes: fused deposition modeling (FDM) in ABS, stereolithography (SLA) in a detailed white resin, and multi-jet fusion (MJF) in polyamide.

Shore Hardness Standards for Cast Polyurethane Parts

Shore hardness is a control number tied to a scale, a temperature, a cure state and a reading time, and a drawing callout needs all four.

Hardness Standards Behind a Cast Polyurethane Shore ValueThree documents appear most often around cast polyurethane. ISO 868 is the plastics method named on the resin sheets, ASTM D2240 is the American test method that reaches rubber and some plastics, and ISO 48-4 is the rubber method that covers softer grades.

Heat Deflection Temperature of Cast Polyurethane Under ISO 75 and ASTM D648

Heat deflection temperature ranks materials under one loaded test and does not set a service ceiling, so it is read together with post-cure and part geometry.

Heat Deflection as One Loaded Bar TestThe test bends a bar under a fixed load while the temperature climbs, and it records the temperature at which the bar has deflected by a set amount. ISO 75-1 describes the general method for determining the temperature of deflection under load, with flexural stress applied in three-point loading.

Silicone Rubber for Vacuum Casting Molds

Mold silicone is an addition-cure rubber chosen for hardness and resin resistance, checked against every material it touches, and treated as a consumable.

Silicone Rubber as the Mold Material in Vacuum CastingA mold silicone is a two-component liquid rubber that is poured round a master, cured at room temperature or a little above, and cut open to release the master. Renishaw describes Vacusil 2000 as a two-component addition-cure liquid silicone rubber designed for mold making, curing at room temperature to a translucent, high-strength elastic rubber, and names vacuum casting of polyurethane resins among its uses.

Clear Polyurethane Casting Resin for Vacuum Casting

A clear polyurethane grade is chosen by section thickness first, and its post-cure has a printed ceiling that protects the color of the part.

How Clear a Casting Resin Is in Datasheet NumbersOn a datasheet, clear is a claim with two numbers behind it at most. PX522 is described as water clear, with a coefficient of light transmission of 89 percent measured by the laboratory LNE, and PX523 prints a refractive index of 1.511.

ABS-Like Polyurethane Casting Resins for Vacuum Casting

An ABS-like polyurethane resin is a stiff thermoset named for its use, and its datasheet numbers depend on post-cure, thickness and test method.

Why a Polyurethane Resin Is Called ABS-LikeThe phrase is a maker's shorthand, not a standard. Sika describes its SikaBiresin PX331 as having mechanical properties similar to thermoplastics like filled ABS, and Renishaw lists its 6230 as having properties similar to ABS.

Send the Drawing of Your Cast Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Vacuum Casting chosen.

Request a Quote