Specimen

A specimen is the test piece a property is measured on, made to the size, thickness and preparation the test method sets.

Every Specimen article of the Vacuum Casting Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A specimen is the test piece a property is measured on, made to the size, thickness and preparation the test method sets. Every value on a casting resin sheet belongs to a specimen of that kind. A cast part matches the printed value only as far as it matches the specimen. Its thickness, cure and conditioning are therefore part of the figure.

Thickness Range

The specimens behind the figures in these resources span a wide range of thickness. Sika’s UL 94 rating for PX331 rests on 3 mm (0.118 in), and its aviation line on 1.5 mm (0.059 in). PX523’s dielectric strength rests on 1 mm (0.039 in). On Renishaw’s sheets, heat deflection uses a 6.4 mm (0.25 in) bar. Shrinkage bars run from 3 mm to 5 mm (0.12 in to 0.20 in). Walls thinner than the specimen fall outside what its figure says.
Read More

Bar Shapes

The Renishaw heat deflection bar is 110 × 12.7 × 6.4 mm (4.33 × 0.50 × 0.25 in). Sika’s sheets give ISO 75A values and name no bar. A shrinkage bar is long and flat on purpose, so the loss is easy to read and the cure stays even. ASTM D648 applies to material 3 mm (0.12 in) or thicker and allows a cemented stack for thinner sheet. ISO 527-1 sets specimen types suited to different materials for tensile tests.

Preparation and Cure

A specimen carries the cure it was given, and the sheets name it in footnotes. ISO 75-2 notes that some materials need annealing of the specimens, which generally raises the result. A post-cured cast specimen behaves the same way. A part delivered without the cure in the footnote is not the specimen of the table.

Specimen Conditioning

Specimens are conditioned before they are tested. ISO 291 sets standard atmospheres for all types of plastics test specimen. UL 94 conditions its vertical bars for 2 days at 23 °C (73 °F) and 50 % relative humidity. Its other conditioning is 7 days at 70 °C (158 °F) in an oven. Whether rated bars and delivered parts share a conditioning history is seldom stated.

Part Difference

A real part differs from a bar in 3 ways the bar hides. A feature around a core cannot shrink freely, a thick section cures hotter, and flow direction changes the result. A 2004 dissertation measured a cast specimen in 8 dimensions with a micrometer reading to 10 µm (0.0004 in). Its losses ranged from 0.29 % to 1.55 % within the one specimen.

Buyer Questions

A buyer working from a sheet asks which specimen produced each figure. The answer names the size, the thickness, the cure and the conditioning. It also says whether the value is measured or typical. Where the part’s wall is thinner than the specimen, a test on the part itself is the direct answer.

Color Matching a Vacuum Cast Batch to a RAL or Pantone Reference

A vacuum cast color is fixed as a weighed recipe on an approved first article, measured with an agreed formula and tolerance, and repeated for every pour.

How a Vacuum Cast Batch Is Matched to a RAL or Pantone ColorA vacuum cast batch is matched to a reference by pigmenting each pour with a paste dosed within the resin maker's limit, casting a first part, measuring it against the reference under agreed conditions, adjusting the recipe, and then holding that recipe for every pour, with parts checked against the approved first article. Renishaw describes the casting system as producing typically 30 to 50 color-matched parts from a single mold, which is the batch size the recipe has to stay steady over.

Flatness and Warp of Large Vacuum Cast Parts

Large vacuum cast panels stay flat through a uniform thin wall, a slow cure, a conformer in post-cure and a temperature kept well below heat deflection.

What Sets Flatness and Warp on a Large Vacuum Cast PartFlatness on a large vacuum cast part is set by five conditions: the heat the resin releases as it cures, the wall thickness against the grade's maximum, how evenly and how long the part cures before demold, whether it is supported during post-cure, and the temperature it later works at. No resin maker, guide or study opened for this piece prints a flatness or warp tolerance for vacuum cast parts.

ISO 527 Tensile Values on Polyurethane Casting Resin Data Sheets

A tensile value on a casting resin sheet belongs to standard bars after one stated cure, so a requirement on parts is set on bars cast and cured with the batch.

What ISO 527 Covers on a Casting Resin Data SheetISO 527 is the international method for tensile properties of plastics, and casting resins fall inside it. The scope of ISO 527-1, as published by the Estonian standards body, sets out the general principles for determining tensile strength, tensile modulus and other aspects of the stress and strain relationship under defined conditions.

ISO 179 and ISO 180 Impact Strength on Cast Resin Data Sheets

Impact values on cast resin sheets are comparisons tied to method, notch, specimen and cure, so a part's toughness is set by tests on batch bars or the part.

What ISO 179 and ISO 180 Measure on a Cast ResinBoth standards measure how much energy a pendulum hammer loses breaking a small bar of plastic at a high strain rate. ZwickRoell, a maker of the testing machines, describes the principle in its pages on both methods: a hammer of specified energy and drop height strikes the specimen, does not swing back to its starting height, and the height difference is taken as the energy absorbed.

PP-Like and PE-Like Polyurethane Casting Resins for Vacuum Casting

PP-like and PE-like urethanes trade stiffness for elongation by grade, and their heat figures depend on cure, so the first cast part is tested in its real duty.

What PP-Like and PE-Like Mean on a Casting Resin Data SheetA PP-like or PE-like grade is a two- or three-component polyurethane formulated so that a part cast in a silicone mold behaves, in hand and in a snap fit, more like polypropylene or polyethylene than like a stiff ABS replica. The makers say so in their own words.

Wall Thickness Limits for Vacuum Cast Polyurethane Parts

Each casting resin carries a maximum thickness printed by its maker, and every property on its sheet describes a specimen of one stated thickness, not the whole part.

Maximum Casting Thickness as the Maker Prints ItSeveral Sika sheets print a line titled maximum casting thickness, and Sika's text for PX522 and PX523 words the same idea as parts until 10 mm or until 100 mm thickness by vacuum casting in silicone molds. Renishaw's resin sheets for 6230 and 8263 print no such line.

Linear Shrinkage of Cast Polyurethane Resins Per 100 mm

Printed shrinkage belongs to one bar and one cure, so the master is scaled from it as a starting point and the first article confirms each critical dimension.

Linear Shrinkage Read as Millimeters Per MeterLinear shrinkage is the fractional loss in length between the mold cavity and the cured part. A resin that fills a cavity 100 mm long and cures into a part that measures 99.3 mm has shrunk by 0.7 percent, which is the same as 7 mm per meter.

Dimensional Accuracy of Vacuum Cast Parts From SLA, FDM and MJF Masters

A cast copy follows its master within a small fraction of a millimeter, and the printed master is the larger source of error against the drawing.

How Accurate Vacuum Cast Parts Are in a Published StudyThe authors cast a battery cover for an enclosure, a thin-walled part 1.5 mm (0.059 in) thick with two measured dimensions: section A at 26.84 mm (1.057 in) and section B at 49.84 mm (1.962 in), both from the CAD model. They made three masters of it by three additive processes: fused deposition modeling (FDM) in ABS, stereolithography (SLA) in a detailed white resin, and multi-jet fusion (MJF) in polyamide.

Heat Deflection Temperature of Cast Polyurethane Under ISO 75 and ASTM D648

Heat deflection temperature ranks materials under one loaded test and does not set a service ceiling, so it is read together with post-cure and part geometry.

Heat Deflection as One Loaded Bar TestThe test bends a bar under a fixed load while the temperature climbs, and it records the temperature at which the bar has deflected by a set amount. ISO 75-1 describes the general method for determining the temperature of deflection under load, with flexural stress applied in three-point loading.

Send the Drawing of Your Cast Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Vacuum Casting chosen.

Request a Quote