ISO 75 is the ISO standard for the temperature of deflection under load of plastics, behind most casting sheets' heat deflection figures.

Every ISO 75 article of the Vacuum Casting Resources, newest first, each written from published standards, research and makers’ data.

Meaning

ISO 75 is the ISO standard for the temperature of deflection under load of plastics, behind most casting sheets’ heat deflection figures. Part 1 gives the general method, with a bar loaded in three-point bending as the temperature rises. Part 2 sets the stress for plastics and ebonite. Sika writes its figures as ISO 75A, and Renishaw states ISO 75 at 1.80 MPa (261 psi).

Loading Methods

ISO 75-2 defines 3 loading methods by the flexural stress on the bar. Method A uses 1.80 MPa (261 psi). Method B uses 0.45 MPa (65 psi), and method C uses 8.00 MPa (1,160 psi). A sheet that prints a heat deflection without the method letter leaves the stress unknown. The 8263 sheet prints its figure without naming a method.
Read More

Stated Limits

Part 1 warns that its results are not necessarily the highest usable temperatures. Service brings other durations, loads and surface stresses than the test. Design calculations and service predictions are outside its purpose. True comparability is reached only between materials with the same room-temperature flexural modulus.

Reproducibility

Part 2 finds amorphous plastics repeat better than semi-crystalline ones. It adds that some materials need annealing of their specimens to give reliable results. Annealing generally raises the measured temperature. A post-cured cast resin behaves the same way, which is why the sheets tie the value to a cure.

Name and Equivalents

Heat distortion temperature is an informal name that no official document adopts. ASTM D648 describes the same idea for molded and sheet materials 3 mm (0.12 in) or thicker. Neither document sets a pass limit, since neither is a specification.

Drawing Statement

A drawing line states grade, ISO 75 method and stress, and the bar’s post-cure. The service temperature the part must survive goes beside them. The first article gets the same cure and a soak at service temperature to prove its shape.

Flatness and Warp of Large Vacuum Cast Parts

Large vacuum cast panels stay flat through a uniform thin wall, a slow cure, a conformer in post-cure and a temperature kept well below heat deflection.

What Sets Flatness and Warp on a Large Vacuum Cast PartFlatness on a large vacuum cast part is set by five conditions: the heat the resin releases as it cures, the wall thickness against the grade's maximum, how evenly and how long the part cures before demold, whether it is supported during post-cure, and the temperature it later works at. No resin maker, guide or study opened for this piece prints a flatness or warp tolerance for vacuum cast parts.

ISO 527 Tensile Values on Polyurethane Casting Resin Data Sheets

A tensile value on a casting resin sheet belongs to standard bars after one stated cure, so a requirement on parts is set on bars cast and cured with the batch.

What ISO 527 Covers on a Casting Resin Data SheetISO 527 is the international method for tensile properties of plastics, and casting resins fall inside it. The scope of ISO 527-1, as published by the Estonian standards body, sets out the general principles for determining tensile strength, tensile modulus and other aspects of the stress and strain relationship under defined conditions.

Rubber-Like Polyurethane Resins From Shore 30 A to 90 A

A rubber-like urethane is specified by grade, hardness method and a tested service temperature, because hardness alone leaves strength and heat behavior open.

Rubber-Like Vacuum Casting Grades and the Hardness Each CoversRubber-like vacuum casting resins are two- or three-component polyurethanes that cure in a silicone mold to an elastomer, with a Shore A hardness chosen for the part. The variable-hardness systems reach the range by adding a third component to a fixed A:B pair.

PP-Like and PE-Like Polyurethane Casting Resins for Vacuum Casting

PP-like and PE-like urethanes trade stiffness for elongation by grade, and their heat figures depend on cure, so the first cast part is tested in its real duty.

What PP-Like and PE-Like Mean on a Casting Resin Data SheetA PP-like or PE-like grade is a two- or three-component polyurethane formulated so that a part cast in a silicone mold behaves, in hand and in a snap fit, more like polypropylene or polyethylene than like a stiff ABS replica. The makers say so in their own words.

When a Vacuum Cast Run Should Move to an Injection Mold

Silicone molds carry a pilot, and a hard tool follows once the quantity, colors and repeat orders outgrow a handful of tools.

Where Silicone Tools Stop and the First Injection Mold StartsInjection molds are rated in classes by the construction they are built to and the cycles they are expected to give. The classification belongs to the plastics industry's trade body, PLASTICS, formerly the Society of the Plastics Industry, and its own text was not opened for this piece.

Demolding and Post-Curing Vacuum Cast Parts

Each grade prints its own demold time and its own post-cure, and thin or long parts are supported in the oven while it runs.

Demolding Vacuum Cast Parts at 70 °CDemolding means opening the silicone tool and taking the copy out once the resin has gelled and hardened far enough to hold its form. In every sheet on file the tool stays at 70 °C (158 °F) in the oven for that time.

Heat Deflection Temperature of Cast Polyurethane Under ISO 75 and ASTM D648

Heat deflection temperature ranks materials under one loaded test and does not set a service ceiling, so it is read together with post-cure and part geometry.

Heat Deflection as One Loaded Bar TestThe test bends a bar under a fixed load while the temperature climbs, and it records the temperature at which the bar has deflected by a set amount. ISO 75-1 describes the general method for determining the temperature of deflection under load, with flexural stress applied in three-point loading.

ABS-Like Polyurethane Casting Resins for Vacuum Casting

An ABS-like polyurethane resin is a stiff thermoset named for its use, and its datasheet numbers depend on post-cure, thickness and test method.

Why a Polyurethane Resin Is Called ABS-LikeThe phrase is a maker's shorthand, not a standard. Sika describes its SikaBiresin PX331 as having mechanical properties similar to thermoplastics like filled ABS, and Renishaw lists its 6230 as having properties similar to ABS.

Send the Drawing of Your Cast Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Vacuum Casting chosen.

Request a Quote