ISO 11359

ISO 11359 is the ISO series for thermomechanical analysis of plastics, used to find a material's thermal expansion and its glass transition temperature.

Every ISO 11359 article of the Vacuum Casting Resources, newest first, each written from published standards, research and makers’ data.

Meaning

ISO 11359 is the ISO series for thermomechanical analysis of plastics, used to find a material’s thermal expansion and its glass transition temperature. Part 2, dated 2021, deals with linear expansion and with the glass transition. Sika cites ISO 11359 for the glass transition on its casting resin sheets. The method follows a small solid specimen’s length as it is heated.

Method Principle

ISO 11359-2 describes thermodilatometry by thermomechanical analysis. The specimen is not loaded in bending, unlike the bar of a heat deflection test. It is also heated differently from an ISO 75 bar. The glass transition it gives and the heat deflection of the same resin therefore need not agree.
Read More

Cited Values

Sika’s sheets give glass transitions under ISO 11359 of 90 °C (194 °F) for PX205 and 95 °C (203 °F) for PX522. PX331 and PX523 both give 100 °C (212 °F). The PX 223 HT sheet gives its expansion coefficient of 115 ppm/°C (64 ppm/°F) under ISO 11359-2. Its glass transition of 120 °C (248 °F) cites a different document, ASTM E1545.

Comparison Across Methods

Renishaw gives the glass transition of 6230 by thermomechanical analysis without naming ISO 11359. The PX331 and 6230 figures are related in method and still come from different sheets. ASTM E1545, a separate standard, can differ by a few degrees on one material. Heat figures compare well only inside one maker’s own sheets.

Drawing Use

A glass transition under ISO 11359 describes the post-cured specimen the footnote names. It does not set a service temperature. A drawing that relies on it names the standard, the cure behind the value and the thermal load the part sees. A soak of the first article at that temperature confirms the part.

Flatness and Warp of Large Vacuum Cast Parts

Large vacuum cast panels stay flat through a uniform thin wall, a slow cure, a conformer in post-cure and a temperature kept well below heat deflection.

What Sets Flatness and Warp on a Large Vacuum Cast PartFlatness on a large vacuum cast part is set by five conditions: the heat the resin releases as it cures, the wall thickness against the grade's maximum, how evenly and how long the part cures before demold, whether it is supported during post-cure, and the temperature it later works at. No resin maker, guide or study opened for this piece prints a flatness or warp tolerance for vacuum cast parts.

ISO 527 Tensile Values on Polyurethane Casting Resin Data Sheets

A tensile value on a casting resin sheet belongs to standard bars after one stated cure, so a requirement on parts is set on bars cast and cured with the batch.

What ISO 527 Covers on a Casting Resin Data SheetISO 527 is the international method for tensile properties of plastics, and casting resins fall inside it. The scope of ISO 527-1, as published by the Estonian standards body, sets out the general principles for determining tensile strength, tensile modulus and other aspects of the stress and strain relationship under defined conditions.

When a Vacuum Cast Run Should Move to an Injection Mold

Silicone molds carry a pilot, and a hard tool follows once the quantity, colors and repeat orders outgrow a handful of tools.

Where Silicone Tools Stop and the First Injection Mold StartsInjection molds are rated in classes by the construction they are built to and the cycles they are expected to give. The classification belongs to the plastics industry's trade body, PLASTICS, formerly the Society of the Plastics Industry, and its own text was not opened for this piece.

Heat Deflection Temperature of Cast Polyurethane Under ISO 75 and ASTM D648

Heat deflection temperature ranks materials under one loaded test and does not set a service ceiling, so it is read together with post-cure and part geometry.

Heat Deflection as One Loaded Bar TestThe test bends a bar under a fixed load while the temperature climbs, and it records the temperature at which the bar has deflected by a set amount. ISO 75-1 describes the general method for determining the temperature of deflection under load, with flexural stress applied in three-point loading.

Clear Polyurethane Casting Resin for Vacuum Casting

A clear polyurethane grade is chosen by section thickness first, and its post-cure has a printed ceiling that protects the color of the part.

How Clear a Casting Resin Is in Datasheet NumbersOn a datasheet, clear is a claim with two numbers behind it at most. PX522 is described as water clear, with a coefficient of light transmission of 89 percent measured by the laboratory LNE, and PX523 prints a refractive index of 1.511.

ABS-Like Polyurethane Casting Resins for Vacuum Casting

An ABS-like polyurethane resin is a stiff thermoset named for its use, and its datasheet numbers depend on post-cure, thickness and test method.

Why a Polyurethane Resin Is Called ABS-LikeThe phrase is a maker's shorthand, not a standard. Sika describes its SikaBiresin PX331 as having mechanical properties similar to thermoplastics like filled ABS, and Renishaw lists its 6230 as having properties similar to ABS.

Send the Drawing of Your Cast Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Vacuum Casting chosen.

Request a Quote